Match the casting defects (Group A) with the probable causes (Group B): GATE ME 2014 Set 3 Production Engineering - Casting Question 51 English
A
$$P - 1,\,\,Q - 3,\,\,R - 2,\,\,S - 4$$
B
$$P - 4,\,\,Q - 3,\,\,R - 2,\,\,S - 1$$
C
$$P - 3,\,\,Q - 4,\,\,R - 2,\,\,S - 1$$
D
$$P - 1,\,\,Q - 2,\,\,R - 4,\,\,S - 3$$
2
GATE ME 2013
MCQ (Single Correct Answer)
+1
-0.3
A cube shaped casting solidifies in $$5$$ min. The solidification time in min for a cube of the same material, which is $$8$$ times heavier than the original casting, will be
A
$$10$$
B
$$20$$
C
$$24$$
D
$$40$$
3
GATE ME 2011
MCQ (Single Correct Answer)
+1
-0.3
Green sand mould indicates that
A
Polymeric mould has been cured
B
Mould has been totally dried
C
Mould is green in colour
D
Mould contains moisture
4
GATE ME 2009
MCQ (Single Correct Answer)
+1
-0.3
Two streams of liquid metal, which are not hot enough to fuse properly, result into a casting defect known as
A
Cold shut
B
Swell
C
Blow hole
D
Scar
GATE ME Subjects
Engineering Mechanics
Machine Design
Strength of Materials
Heat Transfer
Production Engineering
Industrial Engineering
Turbo Machinery
Theory of Machines
Engineering Mathematics
Fluid Mechanics
Thermodynamics
General Aptitude